纳米级锂离子电池正极材料LiFePO4*

梁风** 戴永年 易惠华 熊学

  

  1. ( 昆明理工大学材料与冶金工程学院 真空冶金国家工程实验室 昆明 650093)

  • 收稿日期:2007-11-29 修回日期:2008-03-21 出版日期:2008-10-24 发布日期:2008-10-25
  • 通讯作者: 梁风

Nano-Scale LiFePO4 as Lithium Ion Battery Cathode Materials

Liang Feng** ; Dai Yongnian; Yi Huihua; Xiong Xue

  

  1. (National Engineering Laboratory of Vacuum Metallurgy, Faculty of Materials and Metallurgical Engineering, Kunming University of Science and Technology, Kunming, 650093, China )
  • Received:2007-11-29 Revised:2008-03-21 Online:2008-10-24 Published:2008-10-25
  • Contact: Liang Feng
LiFePO4以其价格便宜,稳定性好,无毒等优点而倍受关注。但是非纳米LiFePO4的电子导电率低及扩散系数小限制了其在锂离子电池领域的大规模应用。而纳米电极材料以其特有的优点很好的解决了这些问题。本文主要综述了国内外合成纳米级LiFePO4 的不同方法及所得材料的对电化学性能和相关机理,以及纳米LiFePO4作为锂离子正极材料存在的问题。
Lithium iron phosphate (LiFePO4 ) has been attracting enomous research interest for its lower cost, high stability, non-toxicity. The extensive use of LiFePO4 in Li-ion batteries is limited by poor electronic conductivity and low lithium ion diffusion limited the application of non-nanos-cale LiFePO4. Nano-scale electrode materials overcome these disadvantages. This paper overcomes chiefly the methods of synthesizing nano-scale LiFePO4, the electrochemical performance of nano-scale LiFePO4, the mechanism of nano-scale LiFePO4 some problems of nano-LiFePO4 as cathode in Li-ion batteries.

中图分类号: 

()

[ 1 ] 吕正中(LüZ Z) , 周震涛(Zhou Z T) . 化学通报(Chemistry) ,2004 , 67 : 79 —84
[ 2 ] 姚耀春( Yao Y C) . 昆明理工大学博士论文(Doctoral Dissertation of Kunming University of Science and Technology) ,2005
[ 3 ] Choi J W, Kim J K, Cheruvally G, et al . J . Power Sources ,2007 , 166 : 211 —218
[ 4 ] Padhi A K, Nanjundaswamy K S , Goodenough J B. J .Electrochem. Soc. , 144(4) : 1188 —1194
[ 5 ] Padhi A K, Nanjundaswamy K S , Masquelier C , et a1. J .Electrochem. Soc. , 1997 , 144 (5) : 1609 —1613
[ 6 ] Yamada A , Chung S C , Hinokuma K. J . Electrochem. Soc. ,2001 , 148 (3) : A224 —A229
[ 7 ] Takahashi M, Ohtsuka H , Akuto K, Sakurai Y. J . Electrochem.Soc. , 2005 , 152 (5) : A899 —A904
[ 8 ] MacNeil D D , Lu Z H , Chen Z H , Dahn J R. J . Power Sources ,2002 , 108 : 8 —14
[ 9 ] Arnold G, Garche J , Hemmer R , Strêbele S , Vogler C ,Wohlfahrt-Mehrens M. J . Power Sources , 2003 , 119P121 : 247 —251
[10] Franger S , le Cras F , Bourbon C , et al . J . Power Sources , 2003 ,119 : 252 —257
[11] Chung S Y, Bloking J T , Chiang YM. Nat . Mater. , 2002 , 2 :123 —128
[12] 李晶泽(Li J Z) . 中国科学院物理研究所博士论文(Doctoral Dissertation of Physics Institute of Chinese Academy of Sciences) ,2000
[13] 田春霞( Tian C X) . 稀有金属( Chinese Journal of Rare Metals) , 2002 , 26(5) : 397 —400
[14] AricòA S , Bruce P , Scrosati B , et al . Nat . Mater. , 2005 , 4 :366 —377
[15] Dominko R , Bele M, Gaberscek M, Remskar M. J . Power Sources , 2006 , 153 : 274 —280
[16] Liu H , Xie J Y, Wang K. Alloys Compd. , 2008 , 456 : 461 —465
[17] Huang H. The Link Foundation Part Ⅰ: Energy (ed. Thompson B J ) . Rochester : University of Rochester , 2003. 19 —34
[18] Choi D , Kumta P N. J . Power Sources , 2007 , 163 : 1064 —1069
[19] Kim D H , KimJ . Phys. Chem. Solids , 2007 , 68 : 734 —737
[20] Kim D H , KimJ . Electrochemical and Solid-State Letters , 2006 ,9 (9) : A439 —A442
[21] Lee J , Teja A S. Mater. Lett . , 2006 , 60 : 2105 —2109
[22] Kim C W, Park J S , Lee K S. J . Power Sources , 2006 , 163 :144 —150
[23] Kim C W, Lee M H , Jeong W T. J . Power Sources. , 2005 ,146 : 534 —538
[24] Kim J K, Choi J W, Cheruvally G, et al . Mater. Lett . , 2007 ,61 : 3822 —3825
[25] Delacourt C , Poizot P , Levasseur S , Masquelier C.Electrochemical and Solid-State Letters , 2006 , 9 ( 7) : A352 —A355
[26] Wang L , Huang Y D , Jiang R R , Jia D Z. Electrochimica Acta ,2007 , 52 : 6678 —6683
[27] Ganesh I , Johnson R , Rao G V N , et al . Ceram. Int . , 2005 ,31 : 67 —74
[28] Wang L N , Zhang Z G, Zhang K L. J . Power Sources , 2007 ,167 : 200 —205
[29] Cao Y L , Yu L H , Li T , Ai X P , Yang H X. J . Power Sources ,2007 , 172 : 913 —918
[30] Wang B F , Qiu Y L , Yang L. Electrochem Commun. , 2006 , 8 :1801 —1805
[31] Prosini P P , Carewska M, Scaccia S , et al . Electrochimica Acta ,2003 , 48 : 4205 —4211
[32] 杨书廷(Yang S T) , 赵娜红(Zhao N H) , 尹艳红(Yi Y H) 等.电池(Battery Bimonthly) , 2005 , 35(4) : 263 —265
[33] Andersson A S , Thomas J O. J . Power Sources , 2001 , 97/98 :498 —502
[34] Singhal A , Skandan G, Amatucci G, et al . Power Sources. ,2004 , 129 : 38 —44
[35] Jamnik J , Maier J . Phys. Chem. Chem. Phys. , 2003 , 5 :5215 —5220
[36] Balaya P , Bhattacharyya A J , Jamnik J , et al . J . Power Sources ,2006 , 159 : 171 —178
[37] Meethong N , Huang H Y S , Carter W C , et al . Electrochemical and Solid-State Letters , 2007 , 10(5) : A134 —A138
[38] Huang H , Yin S C , Nazar L F. Electrochemical and Solid2State Letters , 2001 , 4 (10) : A170 —A172
[39] Wagemaker M, Borghols W J H , Mulder F M. J . Am. Chem.Soc. , 2007 , 129 : 4323 —4327
[40] 石磊(Shi L) . 河南师范大学硕士论文(Master Dissertation of Henan Normal University) , 2006

[1] 刘峻, 叶代勇. 抗病毒涂层[J]. 化学进展, 2023, 35(3): 496-508.
[2] 朱国辉, 还红先, 于大伟, 郭学益, 田庆华. 废旧锂离子电池选择性提锂[J]. 化学进展, 2023, 35(2): 287-301.
[3] 陆峰, 赵婷, 孙晓军, 范曲立, 黄维. 近红外二区发光稀土纳米材料的设计及生物成像应用[J]. 化学进展, 2022, 34(6): 1348-1358.
[4] 周晋, 陈鹏鹏. 二维纳米材料的改性及其环境污染物治理方面的应用[J]. 化学进展, 2022, 34(6): 1414-1430.
[5] 李芳远, 李俊豪, 吴钰洁, 石凯祥, 刘全兵, 彭翃杰. “蛋黄蛋壳”结构纳米电极材料设计及在锂/钠离子/锂硫电池中的应用[J]. 化学进展, 2022, 34(6): 1369-1383.
[6] 王才威, 杨东杰, 邱学青, 张文礼. 木质素多孔碳材料在电化学储能中的应用[J]. 化学进展, 2022, 34(2): 285-300.
[7] 李彬, 于颖, 幸国香, 邢金峰, 刘万兴, 张天永. 手性无机纳米材料圆偏振发光的研究进展[J]. 化学进展, 2022, 34(11): 2340-2350.
[8] 郑明心, 谭臻至, 袁金颖. 光响应Janus粒子体系的构建与应用[J]. 化学进展, 2022, 34(11): 2476-2488.
[9] 漆晨阳, 涂晶. 无抗生素纳米抗菌剂:现状、挑战与展望[J]. 化学进展, 2022, 34(11): 2540-2560.
[10] 王嘉莉, 朱凌, 王琛, 雷圣宾, 杨延莲. 循环肿瘤细胞及细胞外囊泡的纳米检测技术[J]. 化学进展, 2022, 34(1): 178-197.
[11] 赵丹, 王昌涛, 苏磊, 张学记. 荧光纳米材料在病原微生物检测中的应用[J]. 化学进展, 2021, 33(9): 1482-1495.
[12] 陈阳, 崔晓莉. 锂离子电池二氧化钛负极材料[J]. 化学进展, 2021, 33(8): 1249-1269.
[13] 谢勇, 韩明杰, 徐钰豪, 熊晨雨, 王日, 夏善红. 荧光内滤效应在环境检测领域的应用[J]. 化学进展, 2021, 33(8): 1450-1460.
[14] 陆嘉晟, 陈嘉苗, 何天贤, 赵经纬, 刘军, 霍延平. 锂电池用无机固态电解质[J]. 化学进展, 2021, 33(8): 1344-1361.
[15] 高金伙, 阮佳锋, 庞越鹏, 孙皓, 杨俊和, 郑时有. 高电压锂离子正极材料LiNi0.5Mn1.5O4高温特性[J]. 化学进展, 2021, 33(8): 1390-1403.