燃料电池聚合物电解质膜

张宏伟 周震涛   

  1. (华南理工大学材料科学与工程学院 广州 510640)
  • 收稿日期:2007-05-25 修回日期:2007-06-19 出版日期:2008-04-24 发布日期:2008-04-24
  • 通讯作者: 张宏伟

Polymer Electrolyte Membranes for Fuel Cells

Zhang Hongwei; Zhou Zhentao   

  1. (College of Materials Science and Engineering, South China University of Technology, Guangzhou, 510640, PR China)
  • Received:2007-05-25 Revised:2007-06-19 Online:2008-04-24 Published:2008-04-24
  • Contact: Zhang Hongwei
本文简要介绍了聚电解质膜燃料电池的定义、分类、工作原理及其特点,综述了国内外在燃料电池聚电解质领域的最新成果。对质子传导率与甲醇渗透系数的关系进行了初步探讨,详细评述了近年来AAPEM和ACPEM这两类聚电解质膜的研究进展,并对今后的研究趋势作了展望。
This paper presents a brief review of the definition, classification, working principle and characteristic of polymer electrolyte membrane fuel cells and a more detailed review of the progress on polymer electrolyte membranes (PEM) in recent years. Recent developments in the field include acid anionic polymer electrolyte membrane (AAPEM)s such as perfluorosulfonic acid membranes, sulfonated aromatic polymer membranes, sulfonated polyimide membranes, aliphatic hydrocarbon polymer membranes, organic/organic or organic/inorganic composite membranes and alkaline cationic polymer electrolyte membranes (ACPEM). As well, a preliminary description is given of the relation between proton conductivities and methanol permeabilities of AAPEMs. Finally, the further advancements in the area of PEMs are also summarized.

中图分类号: 

()

[ 1 ] Hogarth W H J , da Costa J C D , Lu G Q. Journal of Power Sources , 2005 , 142 : 223 —237
[ 2 ] Oszcipok M, Zedda M, Hesselmann J , et al . Journal of Power Sources , 2006 , 157 : 666 —673
[ 3 ] Mawardi A , Pitchumani R. Journal of Power Sources , 2006 , 160 : 232 —245
[ 4 ] Hickner M A , Ghassemi H , Kim Y S , et al . Chem. Rev. , 2004 , 104 : 4587 —4612
[ 5 ] Varcoe J R , Slade R C T. Fuel Cells , 2005 , 5 (2) : 187 —200
[ 6 ] Wang Y, Li L , Hu L , et al . Electrochemistry Communications , 2003 , 5 : 662 —666
[ 7 ] Slade R C T, Varcoe J R. Solid State Ionics , 2005 , 176 : 585 — 597
[ 8 ] Varcoe J R , Slade R C T, Wright G L , et al . J . Phys. Chem. B , 2006 , 110 : 21041 —21049
[ 9 ] Dicks A L. Journal of Power Sources , 2006 , 156 : 128 —141
[10] Kim J , Kim B , Jung B. Journal of Membrane Science , 2002 , 207 : 129 —137
[11] Guo Q H , Pintauro P N , Tang H , et al . Journal of Membrane Science , 1999 , 154 : 175 —181
[12] Fedkin M V , Zhou X Y, Hofmann M A , et al . Materials Letters , 2002 , 52 : 192 —196
[13] Woo Y, Oh S Y, Kang Y S , et al . Journal of Membrane Science , 2003 , 220 : 31 —45
[14] Yin Y, Fang J H , Cui Y F , et al . Polymer , 2003 , 44 : 4509 — 4518
[15] Elabd Y A , Napadensky E , Sloan J M, et al . Journal of Membrane Science , 2003 , 217 : 227 —242
[16] Gil M, Ji X L , Li X F , et al . Journal of Membrane Science , 2004 , 234 : 75 —81
[17] Li X F , Chen D J , Xu D , et al . Journal of Membrane Science , 2006 , 275 : 134 —140
[18] Binsu V V , Nagarale R K, Shahi V K, et al . Reactive & Functional Polymers , 2006 , 66 : 1619 —1629
[19] Liu B J , Robertson G P , Kim D S , et al . Macromolecules , 2007 , 40 : 1934 —1944
[20] Smitha B , Sridhar S , Khan A A. Journal of Power Sources , 2006 , 159 : 846 —854
[21] Chen W F , Kuo P L. Macromolecules , 2007 , 40 : 1987 —1994
[22] KimB , Kim J , Cha B J , et al . Journal of Membrane Science , 2006 , 280 : 270 —277
[23] Liu B J , Kim D S , Murphy J , et al . Journal of Membrane Science , 2006 , 280 : 54 —64
[24] Wang Z, Ni H Z, Zhao C J , et al . Journal of Membrane Science , 2006 , 285 : 239 —248
[25] Lee K, Nam J D. Journal of Power Sources , 2006 , 157 : 201 — 206
[26] Xue S , Yin G P , Cai KD , et al . J . Membr. Sci . , 2007 , 289 : 51 —57
[27] Son J H , Kang Y S , Won J . Journal of Membrane Science , 2006 , 281 : 345 —350
[28] Zhong S L , Fu T Z, Dou Z Y, et al . Journal of Power Sources , 2006 , 162 : 51 —57
[29] Li X F , Liu C P , Xu D , et al . Journal of Power Sources , 2006 , 162 : 1 —8
[30] Wang Z, Li X F , Zhao C J , et al . Journal of Power Sources , 2006 , 160 : 969 —976
[31] Vishnyakov V M. Vacuum , 2006 , 80 : 1053 —1065
[32] Kariduraganavar M Y, Nagarale R K, Kittur A A , et al . Desalination , 2006 , 197 : 225 —246
[33] Saito M, Arimura N , Hayamizu K, et al . J . Phys. Chem. B , 2004 , 108 : 16064 —16070
[34] Arcella V , Troglia C , Ghielmi A. Ind. Eng. Chem. Res. , 2005 , 44 : 7646 —7651
[35] Bae B , Kim D , Kim HJ , et al . J . Phys. Chem. B , 2006 , 110 : 4240 —4246
[36] Urata S , Irisawa J , Takada A , et al . J . Phys. Chem. B , 2005 , 109 : 17274 —17280
[37] Mauritz KA , Moore R B. Chem. Rev. , 2004 , 104 : 4535 —4585
[38] Weber A Z, Newman J . Chem. Rev. , 2004 , 104 : 4679 —4726
[39] Wang Y Q , Kawano Y, Aubuchon S R , et al . Macromolecules , 2003 , 36 : 1138 —1146
[40] Siu A , Schmeisser J , Holdcroft S. J . Phys. Chem. B , 2006 , 110 : 6072 —6080
[41] Kreuer K D , Paddison S J , Spohr E , et al . Chem. Rev. , 2004 , 104 : 4637 —4678
[42] Kreuer K D. Chem. Mater. , 1996 , 8 : 610 —641
[43] Hensley J E , Way J D. J . Power Sources , 2007 , 172 : 57 —66
[44] Chou J , McFarland E W, Metiu H. J . Phys. Chem. B , 2005 , 109 : 3252 —3256
[45] Pei H Q , Hong L , Lee J Y. Journal of Power Sources , 2006 , 160 : 949 —956
[46] Ioselevich A S , Kornyshev A A , Steinke J H G. J . Phys. Chem. B , 2004 , 108 : 11953 —11963
[47] Silva V S , Mendes A , Madeira L M, et al . Journal of Membrane Science , 2006 , 276 : 126 —134
[48] EikerlingM, Kornyshev A A , Kuznetsov A M, et al . J . Phys. Chem. B , 2001 , 105 : 3646 —3662
[49] Paddison S J , Elliott J A. J . Phys. Chem. A , 2005 , 109 : 7583 —7593
[50] Di Noto V , Gliubizzi R , Negro E , et al . J . Phys. Chem. B , 2006 , 110 : 24972 —24986
[51] Park H S , Kim YJ , Hong W H , et al . Macromolecules , 2005 , 38 : 2289 —2295
[52] Langsdorf B L , Sultan J , Pickup P G. J . Phys. Chem. B , 2003 , 107 : 8412 —8415
[53] Wang H B , de Sousa R , Gasa J , et al . J . Membr. Sci . , 2007 , 289 : 277 —283
[54] Zhu X B , Zhang H M, Zhang Y, et al . J . Phys. Chem. B , 2006 , 110 : 14240 —14248
[55] Tang H L , Pan M, Jiang S P , et al . Electrochimica Acta , 2007 , 52 : 5304 —5311
[56] Adjemian K T, Dominey R , Krishnan L , et al . Chem. Mater. , 2006 , 18 : 2238 —2248
[57] Kim Y, Lee J S , Rhee C H , et al . Journal of Power Sources , 2006 , 162 : 180 —185
[58] Lin Y F , Yen C Y, Ma C CM, et al . Journal of Power Sources , 2007 , 165 : 692 —700
[59] Gosalawit R , Chirachanchai S , Manuspiya H , et al . Catalysis Today , 2006 , 118 : 259 —265
[60] Ekstrom H , Wickman B , Gustavsson M, et al . Electrochim. Acta , 2007 , 52 : 4239 —4245
[61] Kim H , Chang H. J . Membr. Sci . , 2007 , 288 : 188 —194
[62] Kim Y T, Kim K H , Song M K, et al . Current Applied Physics , 2006 , 6 : 612 —615
[63] SaccàA , Gatto I , Carbone A , et al . Journal of Power Sources , 2006 , 163 : 47 —51
[64] Arico A S , Baglio V , di Blasi A , et al . Desalination , 2006 , 199 : 271 —273
[65] Tsuda M, Arboleda N B , Kasai H. Chemical Physics , 2006 , 324 : 393 —397
[66] Zook L A , Leddy J . Anal . Chem. , 1996 , 68 : 3793 —3796
[67] Chen T Y, Leddy J . Langmuir , 2000 , 16 : 2866 —2871
[68] Cho S A , Cho E A , Oh I H , et al . Journal of Power Sources , 2006 , 155 : 286 —290
[69] Drennan J , Webb R , Nogita K, et al . Solid State Ionics , 2006 , 177 : 1649 —1654
[70] Basnayake R , Peterson G R , Casadonte D J , et al . J . Phys. Chem. B , 2006 , 110 : 23938 —23943
[71] Bussian D A , O′Dea J R , Metiu H , et al . Nano Lett . , 2007 , 7 (2) : 227 —232
[72] Sankir M, Bhanu V A , Harrison WL , et al . J . Applied Polymer Science , 2006 , 100 : 4595 —4602
[73] McKay S E , Lashlee R W, Marshall T P , et al . Heteroatom Chemistry , 2005 , 16 (7) : 553 —556
[74] Kreuer KD. Journal of Membrane Science , 2001 , 185 : 29 —39
[75] Roy A , Hickner M A , Yu X, et al . Journal of Polymer Science , Part B : Polymer Physics , 2006 , 44 : 2226 —2239
[76] Pozuelo J , Riande E , Saiz E , et al . Macromolecules , 2006 , 39 : 8862 —8866
[77] Swier S , Gasa J , Shaw M T, et al . Ind. Eng. Chem. Res. , 2004 , 43 : 6948 —6954
[78] Bai Z W, Durstock M F , Dang T D. Journal of Membrane Science , 2006 , 281 : 508 —516
[79] Guan R , Gong C L , Lu D P , et al . Journal of Applied Polymer Science , 2005 , 98 : 1244 —1250
[80] Li C H , Liu J H , Guan R , et al . Journal of Membrane Science , 2007 , 287 : 180 —186
[81] Miyatake K, Shouji E , Yamamoto K, et al . Macromolecules , 1997 , 30 : 2941 —2946
[82] Fujimoto C H , Hicknert M A , Cornelius C J , et al . Macromolecules , 2005 , 38 : 5010 —5016
[83] Aoki M, Chikashige Y, Miyatake K, et al . Electrochemistry Communications , 2006 , 8 : 1412 —1416
[84] Shang X Y, Shu D , Wang S J , et al . Journal of Membrane Science , 2007 , 291 : 140 —147
[85] Tian S H , Shu D , Wang S J , et al . Fuel Cells , 2007 , 7 : 232 — 237
[86] Gao Y, Robertson G P , Guiver MD , et al . Journal of Membrane Science , 2006 , 278 : 26 —34
[87] Chen Y L , Meng Y Z, Hay A S. Macromolecules , 2005 , 38 : 3564 —3566
[88] Chen Y L , Meng Y Z, Wang S J , et al . Macromol . Chem. Phys. , 2006 , 207 : 653 —659
[89] Tian S H , Shu D , Chen YL , et al . Journal of Power Sources , 2006 , 158 : 88 —93
[90] Gu S , He G H , Wu X M, et al . Journal of Membrane Science , 2006 , 281 : 121 —129
[91] Chen H G, Wang S J , Xiao M, et al . J . Power Sources , 2007 , 165 : 16 —23
[92] Zhong S L , Cui X J , Cai H L , et al . Journal of Power Sources , 2007 , 164 : 65 —72
[93] Ding F C , Wang S J , Xiao M, et al . Journal of Power Sources , 2007 , 164 : 488 —495
[94] Xing P X, Robertson G P , Guiver M D , et al . Macromolecules , 2004 , 37 : 7960 —7967
[95] Liu B J , Robertson G P , Guiver M D , et al . Journal of Polymer Science , Part B : Polymer Physics , 2006 , 44 : 2299 —2310
[96] Ge X C , Xu Y, Xiao M, et al . European Polymer Journal , 2006 , 42 : 1206 —1214
[97] Wang L , Meng Y Z, Wang S J , et al . Journal of Polymer Science , Part A: Polymer Chemistry , 2005 , 43 : 6411 —6418
[98] Miyatake K, Oyaizu K, Tsuchida E , et al . Macromolecules , 2001 , 34 : 2065 —2071
[99] Norsten T B , Guiver M D , Murphy J , et al . Adv. Funct . Mater. , 2006 , 16 : 1814 —1822
[100] Kim D S , Robertson G P , Guiver M D , et al . Journal of Membrane Science , 2006 , 281 : 111 —120
[101] Yang Y S , Shi Z Q , Holdcroft S. Macromolecules , 2004 , 37 : 1678 —1681
[102] Gao Y, Robertson G P , Guiver M D , et al . Macromolecules , 2005 , 38 : 3237 —3245
[103] Gao Y, Robertson G P , Kim D S , et al . Macromolecules , 2007 , 40 : 1512 —1520
[104] Zhao C J , Li X F , Wang Z, et al . Journal of Membrane Science , 2006 , 280 : 643 —650
[105] Zhao C J , Lin H D , Shao K, et al . Journal of Power Sources , 2006 , 162 : 1003 —1009
[106] Li X F , Zhang G, Xu D , et al . Journal of Power Sources , 2007 , 165 : 701 —707
[107] Wang L , Meng Y Z, Li X H , et al . Journal of Membrane Science , 2006 , 280 : 108 —115
[108] Zhong S L , Liu C G, Dou Z Y, et al . Journal of Membrane Science , 2006 , 285 : 404 —411
[109] Wang Z, Li X F , Zhao C J , et al . Journal of Applied Polymer Science , 2007 , 104 : 1443 —1450
[110] Wu S Q , Qiu Z M, Zhang S B , et al . Polymer , 2006 , 47 : 6993 —7000
[111] Jouanneau J , Mercier R , Gonon L , et al . Macromolecules , 2007 , 40 : 983 —990
[112] Kim D S , Shin K H , Park H B , et al . Journal of Membrane Science , 2006 , 278 : 428 —436
[113] Schuster M, Kreuer K D , Andersen H T, et al . Macromolecules , 2007 , 40 : 598 —607
[114] Yan Q G, Toghiani H , Causey H. Journal of Power Sources , 2006 , 161 : 492 —502
[115] Basile A , Paturzo L , Iulianelli A , et al . Journal of Membrane Science , 2006 , 281 : 377 —385
[116] Kim H J , Krishnan N N , Lee S Y, et al . Journal of Power Sources , 2006 , 160 : 353 —358
[117] Parcero E , Herrera R , Nunes S P. Journal of Membrane Science , 2006 , 285 : 206 —213
[118] Kìdzierski M, Florjańczyk Z. Journal of Power Sources , 2006 , 159 : 378 —384
[119] Cho C G, Kim Y S , Yu X, et al . Journal of Polymer Science , Part A: Polymer Chemistry , 2006 , 44 : 6007 —6014
[120] Guang R , Dai H , Li C H , et al . Journal of Membrane Science , 2006 , 277 : 148 —156
[121] Li X F , Hao X F , Xu D , et al . Journal of Membrane Science , 2006 , 281 : 1 —6
[122] Pinto B P , Maria L C D , Sena M E. Materials Letters , 2007 , 61 : 2540 —2543
[123] Essafi W, Gebel G, Mercier R. Macromolecules , 2004 , 37 : 1431 —1440
[124] Galatanu A N , Rollet A L , Porion P , et al . J . Phys. Chem. B , 2005 , 109 : 11332 —11339
[125] Rodgers M, Yang Y S , Holdcroft S. European Polymer Journal , 2006 , 42 : 1075 —1085
[126] Asano N , Aoki M, Suzuki S , et al . J . Am. Chem. Soc. , 2006 , 128 : 1762 —1769
[127] Guo X X, Fang J H , Watari T, et al . Macromolecules , 2002 , 35 : 6707 —6713
[128] Ye X H , Bai H , Ho W S W. Journal of Membrane Science , 2006 , 279 : 570 —577
[129] Qiu Z M, Wu S Q , Li Z, et al . Macromolecules , 2006 , 39 : 6425 —6432
[130] Yin Y, Yamada O , Hayashi S , et al . Journal of Polymer Science , Part A: Polymer Chemistry , 2006 , 44 : 3751 —3762
[131] Lee C H , Park H B , Chung Y S , et al . Macromolecules , 2006 , 39 : 755 —764
[132] Jang W, Sundar S , Choi S , et al . Journal of Membrane Science , 2006 , 280 : 321 —329
[133] Hu Z X, Yin Y, Chen S W, et al . Journal of Polymer Science , Part A: Polymer Chemistry , 2006 , 44 : 2862 —2872
[134] Wang L , Yi B L , Zhang H M, et al . Journal of Power Sources , 2007 , 164 : 80 —85
[135] Shi Z Q , Holdcroft S. Macromolecules , 2005 , 38 : 4193 —4201
[136] Chen S L , Benziger J B , Bocarsly A B , et al . Ind. Eng. Chem. Res. , 2005 , 44 : 7701 —7705
[137] Elabd Y A , Napadensky E , Walker C W, et al . Macromolecules , 2006 , 39 : 399 —407
[138] Gubler L , Slaski M, Wokaun A , et al . Electrochemistry Communications , 2006 , 8 : 1215 —1219
[139] Li J Y, Muto F , Miura T, et al . European Polymer Journal , 2006 , 42 : 1222 —1228
[140] Li J Y, Matsuura A , Kakigi T, et al . Journal of Power Sources , 2006 , 161 : 99 —105
[141] Chen J H , Asano M, Maekawa Y, et al . Journal of Membrane Science , 2006 , 277 : 249 —257
[142] Huang H S , Chen C Y, Lo S C , et al . Applied Surface Science , 2006 , 253 : 2685 —2689
[143] Ni H B , Li Z H , Dou H Y, et al . Journal of Fluorine Chemistry , 2006 , 127 : 1036 —1041
[144] Rubatat L , Shi Z Q , Diat O , et al . Macromolecules , 2006 , 39 : 720 —730
[145] Devrim Y G, Rzaev Z M O , Pi©kin E. Macromol . Chem. Phys. , 2006 , 207 : 111 —121
[146] Devrim Y G, Rzaev Z, Piskin E. Macromol . Chem. Phys. , 2007 , 208 : 175 —187
[147] Gao J , Yang Y S , Lee D , et al . Macromolecules , 2006 , 39 : 8060 —8066
[148] Ding J F , Chuy C , Holdcroft S. Macromolecules , 2002 , 35 : 1348 —1355
[149] Deimede V A , Kallitsis J K. Macromolecules , 2005 , 38 : 9594 — 9601
[150] Deimede V , Kandilioti G, Kallitsis J K, et al . Macromol . Symp. , 2005 , 230 : 33 —38
[151] Li X F , Chen D J , Xu D , et al . Journal of Membrane Science , 2006 , 275 : 134 —140
[152] Nagarale R K, Gohil G S , Shahi V K. Journal of Membrane Science , 2006 , 280 : 389 —396
[153] Xue S , Yin G P. Electrochimica Acta , 2006 , 52 : 847 —853
[154] Xue S , Yin G P. Polymer , 2006 , 47 : 5044 —5049
[155] Xue S , Yin G P , Cai KD , et al . J . Membr. Sci . , 2007 , 289 : 51 —57
[156] Kerres J , Tang C M, Graf C. Ind. Eng. Chem. Res. , 2004 , 43 : 4571 —4579
[157] Kerres J , Ullrich A , Hein M, et al . Fuel Cells , 2004 , 4 (1/2) : 105 —112
[158] Kerres J . Fuel Cells , 2005 , 5 (2) : 230 —247
[159] Kerres J . Fuel Cells , 2006 , 6 (3P4) : 251 —260
[160] Mikhailenko S D , Robertson G P , Guiver M D , et al . Journal of Membrane Science , 2006 , 285 : 306 —316
[161] Fu Y Z, Manthiram A , Guiver M D. Electrochemistry Communications , 2006 , 8 : 1386 —1390
[162] Fu Y Z, Manthiram A , Guiver M D. Electrochemistry Communications , 2007 , 9 : 905 —910
[163] Wu X M, He G H , Gu S , et al . Journal of Membrane Science , 2007 , 295 : 80 —87
[164] Lin C W, Huang Y F , Kannan A M. Journal of Power Sources , 2007 , 164 : 449 —456
[165] Burjanadze M, Paulsdorf J , Kaskhedikar N , et al . Solid State Ionics , 2006 , 177 : 2425 —2430
[166] Schauer J , Ku . dela V , Richau K, et al . Desalination , 2006 , 198 : 256 —264
[167] Schauer J , BroˇzováL , Pientka Z, et al . Desalination , 2006 , 200 : 632 —633
[168] Lee J K, Kerres J . Journal of Membrane Science , 2007 , 294 : 75 —83
[169] Xing D , Kerres J . Polym. Adv. Technol . , 2006 , 17 : 591 —597
[170] Mokrini A , Huneault M A. Journal of Power Sources , 2006 , 154 : 51 —58
[171] Mokrini A , Huneault M A , Gerard P. Journal of Membrane Science , 2006 , 283 : 74 —83
[172] Carollo A , Quartarone E , Tomasi C , et al . Journal of Power Sources , 2006 , 160 : 175 —180
[173] Lin H L , Yu TL , Chang W K, et al . Journal of Power Sources , 2007 , 164 : 481 —487
[174] Mitovi S , Vogel B , Roduner E , et al . Fuel Cells , 2006 , 6 (6) : 413 —424
[175] Fu Y Z, Manthiram A. Journal of Power Sources , 2006 , 157 : 222 —225
[176] Deng W Q , Molinero V , Goddard W A Ⅲ. J . Am. Chem. Soc. , 2004 , 126 : 15644 —15645
[177] Subbaraman R , Ghassemi H , Zawodzinski T A. J . Am. Chem. Soc. , 2007 , 129 : 2238 —2239
[178] Sekhon S S , Krishnan P , Singh B , et al . Electrochimica Acta , 2006 , 52 : 1639 —1644
[179] Tigelaar D A , Waldecker J R , Peplowski K M, et al . Polymer , 2006 , 47 : 4269 —4275
[180] Reyna-Valencia A , Kaliaguine S , Bousmina M. Journal of Applied Polymer Science , 2005 , 98 : 2380 —2393
[181] SaccàA , Gatto I , Carbone A , et al . Journal of Power Sources , 2006 , 163 : 47 —51
[182] Ghosh B D , Lott K F , Ritchie J E. Chem. Mater. , 2005 , 17 : 661 —669
[183] Kanamura K, Mitsui T, Munakata H. Chem. Mater. , 2005 , 17 : 4845 —4851
[184] Nagarale R K, Gohil G S , Shahi V K, et al . Macromolecules , 2004 , 37 : 10023 —10030
[185] Ren S Z, Sun G Q , Li C N , et al . Journal of Power Sources , 2006 , 157 : 724 —726
[186] Yamada M, Honma I. J . Phys. Chem. B , 2006 , 110 : 20486 — 20490
[187] Zhang H W, Zhu B K, Xu Y Y. Solid State Ionics , 2006 , 177 : 1123 —1128
[188] Li X F , Xu D , Zhang G, et al . Journal of Applied Polymer Science , 2007 , 103 : 4020 —4026
[189] Shen Y, Qiu X P , Shen J , et al . Journal of Power Sources , 2006 , 161 : 54 —60
[190] Shen J , Xi J Y, Zhu W T, et al . Journal of Power Sources , 2006 , 159 : 894 —899
[191] KimD S , Guiver M D , Nam S Y, et al . Journal of Membrane Science , 2006 , 281 : 156 —162
[192] Kim D S , Yun T I , Seo M Y, et al . Desalination , 2006 , 200 : 634 —635
[193] Brijmohan S B , Shaw M T. Polymer , 2006 , 47 : 2856 —2864
[194] Brijmohan S B , Swier S , Weiss R A , et al . Ind. Eng. Chem. Res. , 2005 , 44 : 8039 —8045
[195] Khiterer M, Loy D A , Cornelius C J , et al . Chem. Mater. , 2006 , 18 : 3665 —3673
[196] Duvdevani T, Philosoph M, Rakhman M, et al . Journal of Power Sources , 2006 , 161 : 1069 —1075
[197] Di Vona M L , D’Epifanio A , Marani D , et al . Journal of Membrane Science , 2006 , 279 : 186 —191
[198] Shahi V K. Solid State Ionics , 2007 , 177 : 3395 —3404
[199] Lu W, Lu D P , Liu J H , et al . Polym. Adv. Technol . , 2007 , 18 : 200 —206
[200] Hill M L , Kim Y S , Einsla B R , et al . Journal of Membrane Science , 2006 , 283 : 102 —108
[201] S« gaard S R , Huan Q , Lund P , et al . Solid State Ion. , 2007 , 178 : 493 —500
[202] Tuckerman M E , Marx D , Parrinello M. Nature , 2002 , 417 : 925 —929
[203] Elattar A , Elmidaoui A , Pismenskaia N , et al . Journal of Membrane Science , 1998 , 143 : 249 —261
[204] Li L , Wang Y X. Journal of Membrane Science , 2005 , 262 : 1 —4
[205] Fang J , Shen P K. Journal of Membrane Science , 2006 , 285 : 317 —322
[206] Zhang H W, Liu X F , Ma X T, et al . Journal of Functional Materials , 2007 , 38 (3) : 412 —414
[207] Wu L , Xu T W, Yang W H. Journal of Membrane Science , 2006 , 286 : 185 —192
[208] Li Y, Xu T W, Gong M. Journal of Membrane Science , 2006 , 279 : 200 —208
[209] Huang A B , Xia C Y, Xiao C B , et al . Journal of Applied Polymer Science , 2006 , 100 : 2248 —2251
[210] Stoica D , Ogier L , Akrour L , et al . Electrochim. Acta , 2007 , 53 : 1596 —1603

[1] 赵秉国, 刘亚迪, 胡浩然, 张扬军, 曾泽智. 制备固体氧化物燃料电池中电解质薄膜的电泳沉积法[J]. 化学进展, 2023, 35(5): 794-806.
[2] 朱月香, 赵伟悦, 李朝忠, 廖世军. Pt基金属间化合物及其在质子交换膜燃料电池阴极氧还原反应中的应用[J]. 化学进展, 2022, 34(6): 1337-1347.
[3] 刘洋洋, 赵子刚, 孙浩, 孟祥辉, 邵光杰, 王振波. 后处理技术提升燃料电池催化剂稳定性[J]. 化学进展, 2022, 34(4): 973-982.
[4] 张旸, 张敏, 赵海雷. 双钙钛矿型固体氧化物燃料电池阳极材料[J]. 化学进展, 2022, 34(2): 272-284.
[5] 占兴, 熊巍, 梁国熙. 从废水到新能源:光催化燃料电池的优化与应用[J]. 化学进展, 2022, 34(11): 2503-2516.
[6] 唐向春, 陈家祥, 刘利娜, 廖世军. 具有三维特殊形貌/纳米结构的Pt基电催化剂[J]. 化学进展, 2021, 33(7): 1238-1248.
[7] 白钰, 王拴紧, 肖敏, 孟跃中, 王成新. 燃料电池用高温质子交换膜[J]. 化学进展, 2021, 33(3): 426-441.
[8] 黄振宇, 涂正凯. 质子交换膜燃料电池电流密度分布特性和研究展望[J]. 化学进展, 2020, 32(7): 943-949.
[9] 张瑞, 吴云, 王鲁天, 吴强, 张宏伟. 微生物燃料电池阴极脱氮[J]. 化学进展, 2020, 32(12): 2013-2021.
[10] 姚东梅, 张玮琦, 徐谦, 徐丽, 李华明, 苏华能. 磷酸掺杂聚苯并咪唑高温膜燃料电池膜电极[J]. 化学进展, 2019, 31(2/3): 455-463.
[11] 叶跃坤, 池滨, 江世杰, 廖世军. 质子交换膜燃料电池膜电极耐久性的提升[J]. 化学进展, 2019, 31(12): 1637-1652.
[12] 梁茜, 王诚, 雷一杰, 刘亚迪, 赵波, 刘锋. 金属有机框架材料在质子交换膜燃料电池中的潜在应用[J]. 化学进展, 2018, 30(11): 1770-1783.
[13] 毛庆*, 景维云, 石越. 非线性谱学分析的基本原理及其在电化学研究中的应用[J]. 化学进展, 2017, 29(2/3): 210-215.
[14] 张文锐, 张智慧, 高立国, 马廷丽. 双钙钛矿型电极材料在中低温固体氧化物燃料电池中的应用[J]. 化学进展, 2016, 28(6): 961-974.
[15] 林玲, 朱青, 徐安武. 直接甲醇燃料电池的阳极和阴极催化剂[J]. 化学进展, 2015, 27(9): 1147-1157.
阅读次数
全文


摘要

燃料电池聚合物电解质膜